Material Notes:
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-running situations, leak-tight material, greater durability, less wear debris – runs cleaner, broader resistance to chemical attack, suitable for fluid and gas applications, lapping of seal face not necessary, and exceptionally stable.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
ASTM-D792
Deformation 10.2 %

@Pressure 13.8 MPa,
Temperature 25.6 °C
10.2 %

@Pressure 2000 psi,
Temperature 78.0 °F
24 hrs.; ASTM-D621
18.3 %

@Pressure 4.14 MPa,
Temperature 260 °C
18.3 %

@Pressure 600 psi,
Temperature 500 °F
24 hrs.; ASTM-D621
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM-D1457
Elongation at Break 175 %
175 %
ASTM-D1457
Flexural Strength 15.2 MPa
2200 psi
ASTM-F417
Flexural Modulus 0.00862 GPa
1.25 ksi
ASTM-D790
Compressive Strength 42.1 MPa
6100 psi
ASTM-C773
Thermal Properties Metric English Comments
CTE, linear 17.8 µm/m-°C
9.90 µin/in-°F
ASTM-D696
Thermal Conductivity 0.692 W/m-K
4.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Descriptive Properties Value Comments
Color Black