Polymer Property : CTE, linear = 17.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 510 Phosphor Bronzes 5% A, Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, Annealed
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C

@Temperature 20.0 - 300 °C
9.90 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 511 Phosphor Bronzes 4%, Spring
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
CTE, linear 17.8 µm/m-°C
9.90 µin/in-°F
ASTM-D696
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
CTE, linear 17.8 µm/m-°C

@Temperature 100 °C
9.89 µin/in-°F

@Temperature 212 °F
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..