Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00862 GPa | 1.25 ksi | ASTM-D790 |
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |