Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 15.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 8960-85 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 916V0 Black PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 9600-85 Clear PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 9940-80 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 9960-85 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM-D1457
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D412
Colorite Polymers CS7541GP Non Lead Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D412
Colorite Polymers CS8039UL Non Lead Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D638
Colorite Polymers MULTICHEM™ 8514 Vinyl-Urethane Blend
Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers.
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D638
Colorite Polymers 7000-UV General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D412
Colorite Polymers CS1542OR Wire and Cable Jacket Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
ASTM D638
Colorite Polymers 7000 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Sylvin Technologies 6149-80 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Copyright © lookpolymers.com All Rights Reserved