Chosun Refractories CUN-198 Nozzle Brick

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CUN-198 Nozzle Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.40 - 2.50 g/cc
0.0867 - 0.0903 lb/in³
Porosity 4.0 - 8.0 %
4.0 - 8.0 %
Mechanical Properties Metric English Comments
Compressive Strength <= 49.0 MPa
<= 7110 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 11.0 - 12.0 µm/m-°C

@Temperature 1000 °C
6.11 - 6.67 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Carbon, C 5.0 - 8.0 %
5.0 - 8.0 %
SiO2 65 - 71 %
65 - 71 %
Descriptive Properties Value Comments
Remarks Ingot casting