Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories AIN-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories COD-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 49.0 MPa | <= 7110 psi | Cold Crushing Strength |
Chosun Refractories CUN-198 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories FSS95 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories GPB-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories H-2 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories SF32 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7100 psi | |
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist .. |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories CH-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories TD-180H Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories H-3S High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 49.0 MPa | 7110 psi | Cold Crushing Strength |
Chosun Refractories TD-165H Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |