Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3) Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria.. |
|||
Bulk Density | 2.40 - 2.70 g/cc | 0.0867 - 0.0975 lb/in³ | |
Reade Advanced Materials Ilmenite Powder (FeTiO3) Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti.. |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
MarkeTech Repton 663 Mullite Brand 663 features: Zirconia.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycle.. |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Sharadaa Ceramics HA 62 High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF60-2 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.40 g/cc | >= 0.0867 lb/in³ | |
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Sharadaa Ceramics REFCAST SUPER Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | >= 2.40 g/cc | >= 0.0867 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 011 Smart Cast Application Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 2.40 g/cc | 0.0868 lb/in³ | Packed |
Excalibar ExBar™ 200 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Bulk Density | 2.40 g/cc | 0.0868 lb/in³ | Packed |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Bulk Density | 2.40 - 2.50 g/cc | 0.0867 - 0.0903 lb/in³ | |
Chosun Refractories BPR-DS Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Chosun Refractories BTB-165 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 - 2.50 g/cc | 0.0867 - 0.0903 lb/in³ | |
Chosun Refractories CUN-198 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 - 2.50 g/cc | 0.0867 - 0.0903 lb/in³ | |
Chosun Refractories CUN-50S Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Chosun Refractories GPB-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Chosun Refractories SAL50 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Chosun Refractories CRAG-L44 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.40 g/cc | 0.0867 lb/in³ | |
Chosun Refractories PCB-TB Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |