Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.40 g/cc
0.0867 lb/in³
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria..
Bulk Density 2.40 - 2.70 g/cc
0.0867 - 0.0975 lb/in³
Reade Advanced Materials Ilmenite Powder (FeTiO3)
Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti..
Bulk Density 2.40 g/cc
0.0867 lb/in³
MarkeTech Repton 663 Mullite
Brand 663 features: Zirconia.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycle..
Bulk Density 2.40 g/cc
0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..
Bulk Density 2.40 g/cc
0.0867 lb/in³
Sharadaa Ceramics HA 62 High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density 2.40 g/cc
0.0867 lb/in³
After Drying at 110°C
Sharadaa Ceramics PCF60-2 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Bulk Density >= 2.40 g/cc
>= 0.0867 lb/in³
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables
Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and ..
Bulk Density 2.40 g/cc
0.0867 lb/in³
Sharadaa Ceramics REFCAST SUPER Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density >= 2.40 g/cc
>= 0.0867 lb/in³
After Drying at 110°C
Sharadaa Ceramics ZAP 011 Smart Cast Application
Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density 2.40 - 2.50 g/cc
0.0867 - 0.0903 lb/in³
Chosun Refractories BPR-DS Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 g/cc
0.0867 lb/in³
Chosun Refractories BTB-165 Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 - 2.50 g/cc
0.0867 - 0.0903 lb/in³
Chosun Refractories CUN-198 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 - 2.50 g/cc
0.0867 - 0.0903 lb/in³
Chosun Refractories CUN-50S Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 g/cc
0.0867 lb/in³
Chosun Refractories GPB-1 Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 g/cc
0.0867 lb/in³
Chosun Refractories SAL50 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 g/cc
0.0867 lb/in³
Chosun Refractories CRAG-L44 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.40 g/cc
0.0867 lb/in³
Chosun Refractories PCB-TB Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).