Thermal Properties Metric English Comments
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C62500 Aluminum Bronze
Finished product available in rods.Chicago Extruded Metal temper code: M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Latrobe LSS™ L6 Tool Steel (ASTM L6)
TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good ..