Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5N-220 Black20.0Di-Cup 40C3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Yield 29.19 MPa
4234 psi
Elongation at Yield 397 %
397 %
100% Modulus 0.00279 GPa
0.405 ksi
200% Modulus 0.009604 GPa
1.393 ksi
300% Modulus 0.02099 GPa
3.045 ksi
Tear Strength 58.3 kN/m
333 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 160 °C
0.250 hour

@Temperature 320 °F