Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 241 - 276 MPa @Strain 0.200 % |
35000 - 40000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 241 - 276 MPa @Strain 0.200 % |
35000 - 40000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 138 - 276 MPa @Strain 0.200 % |
20000 - 40000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | 124 - 276 MPa | 18000 - 40000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, 1/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 193 - 276 MPa | 28000 - 40000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, Annealed Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 110 - 276 MPa | 16000 - 40000 psi | |
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude.. |
|||
Tensile Strength, Yield | 207 - 276 MPa | 30000 - 40000 psi | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300) Allegheny Ludlum's 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |