Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, aged 1000 hours at 982°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, all-weld metal, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, mill annealed Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Indium Corp. Indalloy 27 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Special Metals INCONEL® Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude.. |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals UNS C34000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Density | 8.47 g/cc | 0.306 lb/in³ | |
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |