ChevronTexaco StarFak® PM

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name StarFak® PM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco StarFak® PM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water resistanceExtended relubrication intervalsTexaco Starfak PM is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low temperature conditions and for those difficult applications requiring extended lubrication intervals.It is manufactured using selected highly refined high viscosity synthetic base oils, a lithium complex thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives.The high viscosity index of the synthetic base oils allow for greater pumpability at subzero (-29°C/-20°F) temperatures, allowing bearings lubricated with Texaco Starfak PM to operate at temperatures as low as -51°C (60°F).Texaco Starfak PM grease is recommended for use in applications with temperatures up to 232°C (450°F), with a dropping point of approximately 288°C (550°F). Texaco Starfak PM is ideal for a wide variety of applications across several industries, including:Paper and Forest Products — This grease is suitable for severe service applications such as: sludge press bearings, lime kilns, pumps, woodyard heavy equipment, Doctor oscillator bearings, felt roll bearings, pulp refiner bearings, rope sheaves, and exhaust fan bearings. It is particularly well-suited for the highest temperature applications, such as felt roll bearings and lime kilns operating at temperatures in excess of 204°C (400°F).Mining — Texaco Starfak PM is recommended for: Mining operations that involve extreme pressure applications requiring excellent low temperature pumpability. Applications include: pins and bushings on buckets and loaders, shaker screens, crushers, and conveyors.The lowest temperature mining applications.Automatic lubricating systems in onboard shovels, trucks, and other mobile equipment.Off-Road Construction — This grease is ideally suited for lubrication systems that involve pumping grease through long supply lines at low temperatures. It also displays superior water washout resistance properties in wet, off-road environments.Steel — Steel mill applications often involve extremely high temperatures. The excellent structural stability of Texaco Starfak PM makes it appropriate in these situations. Its extreme pressure properties and superior resistance to water washout are also key in the steel mill environment. This grease provides outstanding protection for steel mill roll bearings, conveyors, furnace and coiler grease points, pump bearings, and exhaust fan bearings.Marine — The rust and corrosion inhibition properties of Texaco Starfak PM makes it ideal for use in marine equipment exposed to severe corrosion environments. Examples include deck equipment, offshore drilling equipment, grease lubricated shaft bearings, cranes, and windlass winches. Texaco Starfak PM is approved for the NLGI certification mark LB.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 222657; MSDS Number: 8841
Physical Properties Metric English Comments
Viscosity Measurement 148
148
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1791 SUS
1791 SUS
See Note 3.
Saybolt Viscosity at 210°F 172 SUS
172 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 344 cSt
344 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 35.5 cSt
35.5 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 79
79
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
Four Ball Wear 0.260 mm
0.0102 in
Scar Diameter
Penetration P(0), 1/10 mm 295
295
Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 315
315
Unknown Amount of Work, 25°C (77°F)
Timken Test 22700 g
50.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 235 °C
455 °F
See Note 2.
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
See Note 1.
Flash Point 280 °C
536 °F
See Note 3.
Dropping Point 312 °C
594 °F
Descriptive Properties Value Comments
Bearing Water Washout, wt% 5
Loss at 175°F
Color Light Tan
Corrosion, Copper Strip 1B
Texture Smooth, Buttery
Thickener, % 13
Lithium Complex