Flash Point 280 °C
536 °F
COC Method; JIS K 2265
Mitsui LUCANTâ„¢ HC-100 Synthetic Oil
LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity..
Flash Point 280 °C
536 °F
ASTM D92
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Flash Point 280 °C
536 °F
[°C] Fire Point
ChevronTexaco Canopus® 100
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Flash Point 280 °C
536 °F
ChevronTexaco Quenchtex® MM
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f..
Flash Point 280 °C
536 °F
See Note 3.
ChevronTexaco Thermatex® EP NLGI Grade 1
Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub..
Flash Point 280 °C
536 °F
See Note 3.
ChevronTexaco Thermatex® EP NLGI Grade 2
Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub..
Flash Point 280 °C
536 °F
ASTM D92
ExxonMobil Mobil Vaculine 128
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Flash Point 280 °C
536 °F
COC
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40
Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and..
Flash Point 280 °C
536 °F
COC
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 40
Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t..
Flash Point 280 °C
536 °F
ASTM D92
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Flash Point 280 °C
536 °F
See Note 3.
ChevronTexaco StarFak® PM
Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water ..
Flash Point 280 °C
536 °F
ASTM D92
ChevronTexaco Ulti-Plex® Synthetic Grease EP
FeaturesChevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low ..
Flash Point 280 °C
536 °F
COC
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 30
Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t..
Flash Point 280 °C
536 °F
ASTM D92
ExxonMobil Mobil Vaculine 128
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..