Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 172 SUS
172 SUS
See Note 3.
ChevronTexaco StarFak® PM
Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water ..
Saybolt Viscosity at 210°F 172 SUS
172 SUS
ChevronTexaco Ulti-Plex® Synthetic Grease EP
FeaturesChevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low ..