FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybdenum disulfide (moly), EP additive, rust and oxidation inhibitors. They are dark gray/black in color and smooth and buttery in texture.These products satisfy the demand for high quality moly-type greases with extreme pressure capability in both automotive and industrial applications.Chevron Moly Greases EP provide excellent performance under extreme pressure, boundary lubrication conditions because of their EP additive and moly content. With a Timken OK Load (ASTM D 2509) of 50 lbs and moly to maintain a low coefficient of friction along sliding surfaces, even under loads exceeding the yield strengths of metals, Chevron Moly Greases EP provide both shock and heavy load protection. Moly provides a lubricity safety factor (staying power) in situations where the grease is depleted and only molybdenum disulfide remains to provide lubrication until more grease is applied.Chevron Moly Greases EP provide longer-lasting lubrication than conventional greases. Hence, lubrication frequencies can be extended and down time reduced. They are ideal in situations where lubrication is infrequent. The "moly" provides a reserve protection should the lubricant be squeezed from the bearing surface. They have good storage stability, are pumpable at low temperatures, and provide water resistance and rust protection.ApplicationsChevron Moly Greases EP are recommended for use in automotive and industrial equipment where a moly type grease is called for.Typical applications in automotive equipment are: chassis, bearings, universal joints, fifth wheels, and ball joints in construction equipment such as bulldozers, scrapers, loaders, shovels, etc.Chevron Moly Greases EP are recommended for use in roller chains, trunions, gears, cables, sheaves, slides, and chassis bearings.In industrial applications, these greases are recommended for the lubrication of conveyor bearings, sliding and rubbing surfaces, kiln car bearings, etc. They are particularly suited for heavily loaded pivot pins, splined shafts, or other surfaces subjected to sliding, vibration, or oscillation where fretting is encountered.Chevron Moly Greases EP meet Caterpillar recommendations for greases containing 3% molybdenum disulfide.
Physical Properties Metric English Comments
Viscosity Measurement 53
53
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1074 SUS
1074 SUS
Saybolt Viscosity at 210°F 77 SUS
77 SUS
Kinematic Viscosity at 40°C (104°F) 200 cSt
200 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.2 cSt
14.2 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Point
Penetration 280
280
Worked
Penetration P(0), 1/10 mm 275
275
Timken Test 22700 g
50.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 127 °C
261 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Pour Point -18.0 °C
-0.400 °F
ASTM D97
Flash Point 249 °C
480 °F
ASTM D92
Dropping Point 191 °C
376 °F
Descriptive Properties Value Comments
Color Dark Gray/Black
Lincoln Ventmeter, psig at 30 s, at 0°F 583
Lincoln Ventmeter, psig at 30 s, at -22°F 1367
Lincoln Ventmeter, psig at 30 s, at 75°F 400
Texture Smooth, Buttery
Thickener, % / type 6.4 / Lithium