Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | ASTM D445 |
ChevronTexaco NLGI 1 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | ASTM D445 |
ChevronTexaco NLGI 2 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | Base Oil |
ConocoPhillips 2 Super Lube M EP Grease NLGI No. Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road.. |
|||
Kinematic Viscosity at 40°C (104°F) | 200 cSt | 200 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368S (RL) Synthetic Oil Information provided by Nye Lubricants. |