Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for additional greases throughout the plant.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.Determined on mineral oil extracted by vacuum filtration.Unknown amount of workCPS Number: 221932; MSDS Number: 9002
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1178 SUS
1178 SUS
See Note 3.
Saybolt Viscosity at 210°F 84 SUS
84 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
See Note 3.
Oxidative Stability 100 hour
100 hour
Drop, 10 psi max; ASTM D942
Mechanical Properties Metric English Comments
Penetration 5.0
5.0
% Change, (10000X), 25°C, See Note 4.
Penetration P(60), 1/10 mm 325
325
Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g
40.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
Minimum Service Temperature, Air -23.0 °C
-9.40 °F
See Note 1.
Flash Point 190 °C
374 °F
See Note 3.
Dropping Point 221 °C
430 °F
Descriptive Properties Value Comments
Color Brown
Texture Smooth
Thickener, % 8
Aluminum Complex