ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear® Wet Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality, hydrocracked base oil, combined with a specially tailored additive package and oiliness agent, provides resistance to oil wash off from cylinders in “wet gas” compression service. Moreover, Wet Gas Compressor Fluid can be used in reciprocating compressor crankcases that call for nondetergent oils. Note: The interaction between natural gas and hydrocarbon-based oils can lead to an effect known as ”gas dilution.” This effect reduces the effective viscosity of the lubricant and is normally taken into account by using ISO 220 viscosity grade products. Experience has shown that Hydroclear Wet Gas Compressor Fluid provides excellent service and value in applications for which the specific gravity of the gas stream is less than 1.0 and the gas outlet temperatures are well above the condensation point of the gas.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
60°F
Viscosity Measurement 97
97
Viscosity Index
Saybolt Viscosity at 100°F 1150 SUS
1150 SUS
Saybolt Viscosity at 210°F 95 SUS
95 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
Kinematic Viscosity at 100°C (212°F) 18.5 cSt
18.5 cSt
Oxidative Stability 4000 hour
4000 hour
Oxidation Resistance; ASTM D943
Mechanical Properties Metric English Comments
Four Ball Wear 0.400 mm
0.0157 in
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 285 °C
545 °F
Descriptive Properties Value Comments
ASTM Rust A&B Pass
Copper Corrosion 1A
FZG Pass 9 Load Stages
ASTM D5182