Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 84 SUS
84 SUS
See Note 3.
ChevronTexaco EP 1 Aluminum Complex
Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for addition..