Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density PolyethyleneCustomer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE.Applications: Merchandise bags, linersProperty Comments: LLDPE line, 2.5:1 BUR, .08" diegap, 8" die, 56" FLH, 250 lbs/hr, 400°FData provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.933 g/cc
0.0337 lb/in³
ASTM D1505
Melt Flow 0.70 g/10 min
0.70 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.420 GPa
60.9 ksi
at 1%; ASTM D882
Secant Modulus, TD 0.460 GPa
66.7 ksi
at 1%; ASTM D882
Coefficient of Friction, Dynamic 0.60
0.60
ASTM D1894
Coefficient of Friction, Static 0.70
0.70
ASTM D1894
Elmendorf Tear Strength MD 45 g
45 g
ASTM D1922
Elmendorf Tear Strength TD 280 g
280 g
ASTM D1922
Dart Drop Test 120 g
0.265 lb
26 in; ASTM D1709
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 66 %
66 %
45°; ASTM D2457
Descriptive Properties Value Comments
Process Film
Region Mexico
Bamberger Polymers Distribution