Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.420 GPa | 60.9 ksi | at 1%; ASTM D882 |
Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE.Applic.. |