Material Notes:
A modified injection molding grade nylon for applications requiring flexibility.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ATSM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Modulus 0.810 GPa
117 ksi
ASTM D790
Izod Impact, Notched 1.98 J/cm
3.71 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648