Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Higher melt flow index compared with other grades; good balance of modulus and toughness. Applications requiring complicated structure or thin wall thickness.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 12 - 15 g/10 min
12 - 15 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ISO 868
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ISO 527-1
Elongation at Break 500 %
500 %
ISO 527-1
Flexural Modulus 0.204 GPa
29.6 ksi
ISO 178
Tear Strength 150 kN/m
856 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 203 °C
397 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974