Material Notes:
Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following product profile: Very high stiffness and strengthExcellent impact and notched impact strength Very low moisture absorptionSuitable for often repeated steam sterilizationVery high dimensional stabilityEasy processing, good flow, characteristicsHigh molding precision, low warpage Grilamid LVX-65H SST natural is suitable for production of technical parts in applications such as: Electronic devicesAutomotiveMechanical engineeringSafety componentsMedical devices and instrumentsSports and Leisure goodsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Water Absorption 0.80 %
0.80 %
ISO 62
Moisture Absorption 0.400 %
0.400 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 200 MPa
29000 psi
conditioned; ISO 2039-1
Tensile Strength at Break 185 MPa
26800 psi
conditioned; ISO 527-1/-2
210 MPa
30500 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
2.5 %
2.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 17.0 GPa
2470 ksi
conditioned; ISO 527-1/-2
19.0 GPa
2760 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
dry; ISO 179/1eA
2.50 J/cm²
11.9 ft-lb/in²
conditioned; ISO 179/1eA
2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 43.0 kV/mm
1090 kV/in
dry; IEC 60243-1
43.0 kV/mm
1090 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Hydraulic systems
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sanitary, water and gas supply
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)