Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blend of H3303 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and flame retardancy, such as wires, cables and optical fiber.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Melt Flow 5.0 - 10 g/10 min
5.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ISO 868
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ISO 527-1
Elongation at Break 350 %
350 %
ISO 527-1
Flexural Modulus 0.0450 GPa
6.53 ksi
ISO 178
Tear Strength 55.0 kN/m
314 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Brittleness Temperature -60.0 °C
-76.0 °F
ISO 974