Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast unoriented film extrusion and for injection molding of articles that need good mold release properties. CAPILENE® QM 45 F is also used in blends with CAPILENE® QM 50 F, M 45 F, and M 50 F.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 9.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ASTM D638
Elongation at Yield 15 %
15 %
50 mm/min; ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 132 °C

@Load 1.02 kg
270 °F

@Load 2.25 lb
ASTM D1525
Optical Properties Metric English Comments
Haze 2.0 %

@Thickness 0.0400 mm
2.0 %

@Thickness 0.00157 in
ASTM D1003