Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87707 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -20.0 °C |
0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.656 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | >= 0.350 J/cm @Temperature -20.0 °C |
>= 0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8300N Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | >= 0.350 J/cm @Temperature -20.0 °C |
>= 0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8332M (EPC40R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -20.0 °C |
0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010RV PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0360 T8 Polypropylene, 30% Mineral Filled PP homopolymer 30% mineral fillerExtrusion gradeInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -20.0 °C |
0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 141 Injection Molding Polypropylene Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem RP 144 Coating Polypropylene Description: RP 144 is a high melt flow rate random copolymer, designed for high speed coating equipments. This product features good processability, excellent gloss and weldability.Applications: Wa.. |