Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.19 µm/m-°C @Temperature 20.0 °C |
6.772 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |