Thermal Properties Metric English Comments
Thermal Conductivity 13.7 W/m-K
95.1 BTU-in/hr-ft²-°F
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367)
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 30% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 60% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Thermal Conductivity 13.7 W/m-K

@Temperature 20.0 - 100 °C
95.1 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..