Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 1380 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Alloy 436 Platinum/Tungsten Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Alloy 436L Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1380 MPa
200000 psi
Hard
California Fine Wire Stablohm 875 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.