Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds HGK 79 Flexible PVC, Sheathing for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HGK 79 Flexible PVC, Sheathing for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheathing oil and hydrocarbon resistent
Physical Properties Metric English Comments
Density 1.35 - 1.39 g/cc
0.0488 - 0.0502 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 81
77 - 81
ISO R 868
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
ISO R 527
Elongation at Break >= 300 %
>= 300 %
ISO R 527
Descriptive Properties Value Comments
Thermal Stability (minutes) 300
CEI 20-34/3-2