Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | >= 1100 °C | >= 2010 °F | Fiber |
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |
|||
Melting Point | >= 1100 °C | >= 2010 °F | Fiber |
Tritex TREO Needled Blanket Insulation Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries.. |
|||
Melting Point | 1100 °C | 2012 °F | |
California Fine Wire Copper, 27% Nickel Clad All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1100 °C | 2012 °F | |
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1100 °C | 2012 °F | |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1100 °C | 2012 °F | |
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1100 °C | 2012 °F | |
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |