Material Notes:
For vacuum switch contacts.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 17.17 g/cc
0.6203 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 27
27
Flexural Modulus 1.24 GPa
180 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 115 W/m-K
798 BTU-in/hr-ft²-°F
Melting Point 1080 - 3410 °C
1980 - 6170 °F
Solidus 1080 °C
1980 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Copper, Cu 10 %
10 %
Tungsten, W 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000493 ohm-cm
0.00000493 ohm-cm
(35% IACS)