CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer CMW Inc.
Trade Name ELKALOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility. In the ELKALOY® D alloy impurities (including iron) are kept low to obtain maximum electrical thermal conductivity.ELKALOY® D130 material is recommended for extremely heavy duty applications where ELKALOY® D, ELKALOY® D110, and ELKALOY® D120 materials proved too low in mechanical properties. In addition, it is used for guideposts, bushings, forming die rings and inserts, wiping blocks and forming tools where no impact is involved. It is especially good in forming stainless steel.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 7.20 g/cc
0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 35
35
Tensile Strength, Ultimate 586 MPa
85000 psi
Tensile Strength, Yield 483 MPa
70100 psi
Elongation at Break 0.50 %
0.50 %
Reduction of Area 0.00 %
0.00 %
Modulus of Elasticity 103 GPa
14900 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 67.0 W/m-K
465 BTU-in/hr-ft²-°F
Melting Point 1025 - 1060 °C
1877 - 1940 °F
Solidus 1025 °C
1877 °F
Liquidus 1060 °C
1940 °F
Component Elements Properties Metric English Comments
Aluminum, Al 14 %
14 %
Beryllium, Be 0.50 %
0.50 %
Co + Ni 1.5 - 2.55 %
1.5 - 2.55 %
Copper, Cu 78.55 - 79.4 %
78.55 - 79.4 %
Iron, Fe 4.6 %
4.6 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000192 ohm-cm
0.0000192 ohm-cm
9 % IACS