Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Melting Point | 1025 - 1060 °C | 1877 - 1940 °F | |
CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Melting Point | 1025 - 1060 °C | 1877 - 1940 °F | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Melting Point | 1025 - 1060 °C | 1877 - 1940 °F | |
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Melting Point | 1025 - 1060 °C | 1877 - 1940 °F | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Melting Point | 1040 - 1060 °C | 1900 - 1940 °F | |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |