Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 67.0 W/m-K @Temperature 85.0 °C |
465 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 3 In-Ag Solder Alloy Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 3444 0 Annealed Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter > 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Thermal Conductivity | 67.0 W/m-K | 465 BTU-in/hr-ft²-°F | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |