Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 103 GPa | 15000 ksi | |
H.C. Starck Pure Niobium (Columbium) Applications: NRC® niobium metal is produced from electron beam melted ingots. Grain Stabilized Niobium (GSNb) is made by EB and VAR melting. Both materials are malleable, weldable, machineabl.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
Schott N-KZFS8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4987.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Modulus of Elasticity | 103 - 110 GPa | 14900 - 16000 ksi | Typical |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
Wieland BioPorta G PFM Alloy Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
Wieland Porta Aurium PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Modulus of Elasticity | 103 GPa @Temperature 299 °C |
15000 ksi @Temperature 570 °F |
|
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |
|||
Modulus of Elasticity | 103 GPa | 14900 ksi | |
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |
|||
Modulus of Elasticity | 103 GPa @Temperature 600 °C |
15000 ksi @Temperature 1110 °F |
|
Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel Magnadie-RF is a premium quality 5% chromium hot work die steel. The chemistry of Magnadie-RF steel is a modification of the premium quality H-13 chemistry. Magnadie-RF steel is designed for incre.. |