Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 CX105 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Temperature Coefficient of 0.0017/K |
Goodfellow Platinum 94/Rhodium 6 Thermocouple Alloy Information provided by Goodfellow. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | 9 % IACS |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Electrical Resistivity | 0.0000192 ohm-cm | 0.0000192 ohm-cm | Conductivity is 9% IACS |
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |