Material Notes:
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility. In the ELKALOY® D alloy impurities (including iron) are kept low to obtain maximum electrical thermal conductivity.ELKALOY® D material is recommended for certain flash welding operations, particularly for cold rolled steel and stainless set. The entire die is made from ELKALOY® D material. ELKALOY® D material is also used as a backing on barrel welding dies, faced with either CMW® 73 or ELKONITE® materials. The material may be used as an inexpensive current carrying member for welders or welding jigs, fixtures, or dies where high electrical conductivity is not of prime importance. Typical examples of welder arms, knees, platens and die and fixture bases.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 75
75
Tensile Strength, Ultimate 438 MPa
63500 psi
Tensile Strength, Yield 207 MPa
30000 psi
Elongation at Break 8.0 %
8.0 %
Reduction of Area 8.0 %
8.0 %
Modulus of Elasticity 103 GPa
14900 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 67.0 W/m-K
465 BTU-in/hr-ft²-°F
Melting Point 1025 - 1060 °C
1877 - 1940 °F
Solidus 1025 °C
1877 °F
Liquidus 1060 °C
1940 °F
Component Elements Properties Metric English Comments
Aluminum, Al 10 %
10 %
Beryllium, Be 0.50 %
0.50 %
Co + Ni 1.5 - 2.55 %
1.5 - 2.55 %
Copper, Cu 86.95 - 88 %
86.95 - 88 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000960 ohm-cm
0.00000960 ohm-cm
18 % IACS