Radici Raditer® BRV300 Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Raditer® BRV300 Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT Glass Fiber ReinforcedInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 125 MPa
18100 psi
ISO 527-1/2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/2
Tensile Modulus 10.15 GPa
1472 ksi
ISO 527-1/2
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 7.50 GPa
1090 ksi
ISO 178
Charpy Impact Unnotched 6.60 J/cm²
31.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75/2Af
Vicat Softening Point 210 °C
410 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in