Material Notes:
For electrical contacts.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.33 g/cc
0.3732 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 35 - 89
35 - 89
35 (annealed) - 89 (worked)
Tensile Strength, Ultimate 172 MPa
24900 psi
Annealed
290 MPa
42100 psi
Worked
Thermal Properties Metric English Comments
Melting Point <= 1453 °C
<= 2647 °F
Liquidus 1453 °C
2647 °F
Component Elements Properties Metric English Comments
Nickel, Ni 10 %
10 %
Silver, Ag 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000198 ohm-cm
0.00000198 ohm-cm
(87% IACS)