Thermal Properties Metric English Comments
Liquidus 1453 °C
2647 °F
CMW® D50 Silver Nickel Contact Material ASTM B693
For electrical contacts; resistant to mechanical wear.Information provided by CMW Inc.
Liquidus 1453 °C
2647 °F
CMW® D510F Silver Nickel Contact Material ASTM B693
For electrical contacts.Information provided by CMW Inc.
Liquidus 1453 °C
2647 °F
CMW® D56 Silver Nickel Contact Material B693
For electrical contacts; resistant to mechanical wearInformation provided by CMW Inc.
Liquidus 1453 °C
2647 °F
CMW® D505F Silver Nickel Contact Material
For electrical contacts.Information provided by CMW Inc.