Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 290 MPa
42000 psi
Typical
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Ultimate 290 MPa
42000 psi
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Ultimate 290 MPa
42000 psi
ASTM D638
RTP Company RTP 4086  Polyphthalamide (PPA) Carbon Fiber 35%  (discontinued **)
Carbon Fiber 35%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Tensile Strength, Ultimate >= 290 MPa
>= 42100 psi
H.C. Starck MoCu 70/30 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
Tensile Strength, Ultimate 290 MPa

@Temperature 980 °C
42100 psi

@Temperature 1800 °F
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 290 MPa

@Temperature 870 °C
42100 psi

@Temperature 1600 °F
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Ultimate 290 MPa
42000 psi
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Strength, Ultimate 290 MPa
42000 psi
MTI ThermoStran® PPA-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Strength, Ultimate 290 MPa

@Temperature 980 °C
42100 psi

@Temperature 1800 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 290 MPa

@Temperature 870 °C
42100 psi

@Temperature 1600 °F
Haynes Hastelloy® alloy X 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Ultimate 290 MPa
42000 psi
Transverse
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed
Data provided by the manufacturer, Special Metals.
Tensile Strength, Ultimate 290 - 359 MPa
42000 - 52000 psi
Eagle Brass 210 Gilding Metal, 1/2 Hard
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Ultimate 290 MPa
42100 psi
ACMA Test #4
CoorsTek Zirconia-Toughened Alumina, ZTA
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Tensile Strength, Ultimate 290 MPa
42100 psi
Worked
CMW® D510F Silver Nickel Contact Material ASTM B693
For electrical contacts.Information provided by CMW Inc.
Tensile Strength, Ultimate >= 290 MPa
>= 42100 psi
AK Steel Grade 25 Cold Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Tensile Strength, Ultimate 290 MPa
42000 psi
Ametek P316L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density
P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu..
Tensile Strength, Ultimate 290 MPa
42100 psi
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.35 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Tensile Strength, Ultimate 290 MPa
42100 psi
Rm
ALIMEX ACP 5080 Aluminum Cast Plate
ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum..
Tensile Strength, Ultimate 290 MPa
42100 psi
Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.38 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Tensile Strength, Ultimate 290 MPa

@Thickness 5.00 - 12.0 mm
42100 psi

@Thickness 0.197 - 0.472 in
Typical L-T Direction
Aleris HOGAL 5558 Aluminum 5026 H14/H34
HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris.
Tensile Strength, Ultimate 290 MPa
42100 psi
Rm
ALIMEX ACP 5080R Aluminum Cast Material
Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information ..