Polymer Property : Tensile Strength, Ultimate = 24900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 172 MPa
24900 psi
ISO value at 5mm/min.
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
Tensile Strength, Ultimate 172 MPa
24900 psi
DIN 53455; ASTM D638
Kolon KOPA® KN133G33SIBL G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 172 MPa
24900 psi
DIN 53455; ASTM D638
Kolon KOPA® KN332G30VO G/F Reinforced & Flame Retardant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 172 MPa
24900 psi
DIN 53455; ASTM D638
Kolon KOPA® KN133G30 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 172 MPa
24900 psi
Sawbones Second-Generation Simulated Cortical Bone
E-glass / Epoxy CompositeSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ..
Tensile Strength, Ultimate 172 MPa
24900 psi
ASTM D638
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac..
Tensile Strength, Ultimate 172 MPa
24900 psi
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Tensile Strength, Ultimate 172 MPa
24900 psi
Annealed
CMW® D510F Silver Nickel Contact Material ASTM B693
For electrical contacts.Information provided by CMW Inc.
Tensile Strength, Ultimate 172 MPa
24900 psi
Annealed
CMW® D582F Silver Graphite Contact Material
For electrical contacts; reduced sticking, low voltage DCInformation provided by CMW Inc.
Tensile Strength, Ultimate 172 MPa
24900 psi
ISO value at 5mm/min.
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista..