Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1453 °C | 2647 °F | |
CMW® D50 Silver Nickel Contact Material ASTM B693 For electrical contacts; resistant to mechanical wear.Information provided by CMW Inc. |
|||
Liquidus | 1453 °C | 2647 °F | |
CMW® D510F Silver Nickel Contact Material ASTM B693 For electrical contacts.Information provided by CMW Inc. |
|||
Liquidus | 1453 °C | 2647 °F | |
CMW® D56 Silver Nickel Contact Material B693 For electrical contacts; resistant to mechanical wearInformation provided by CMW Inc. |
|||
Liquidus | 1453 °C | 2647 °F | |
CMW® D505F Silver Nickel Contact Material For electrical contacts.Information provided by CMW Inc. |