CEN® Electronic Material HT Polyimide Film

Category Polymer , Thermoset , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer CEN® Electronic Material Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CEN® Electronic Material HT Polyimide Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CEN® HT is a one side or both sides electrically conductive polyimide film for heating applications. With precisely controlled surface resistivity, the film resistive property is retained throughout the film, so it cannot be cracked, rubbed off or easily damaged, as is often the case with surface coatings or metallizations.Applications: heaters, heating facilities for automotive, health care, agriculture, aerospace, and consumer electronics.All information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Thickness 46.0 - 54.0 microns
1.81 - 2.13 mil
ASTM D374
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 110 MPa
16000 psi
ASTM D882
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882
Elongation at Yield >= 10 %
>= 10 %
ASTM D882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D257
Processing Properties Metric English Comments
Shelf Life >= 1.25 Month
>= 1.25 Month
Descriptive Properties Value Comments
Folding Endurance >500,000 times
Power Density (W/cm²) 6
Rate of Electricity to Thermal (%) >99
Tolerance of Resistance (%) <3
Working Voltage (V) 3-850