Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 46.0 - 54.0 microns | 1.81 - 2.13 mil | ASTM D374 |
CEN® Electronic Material BX Polyimide Film CEN®BX Polyimide Film are electrically conductive, and are precisely loaded with conductive fillers to produce films with tightly controlled surface resistivities. BX films provide both thermal and.. |
|||
Thickness | 46.0 - 54.0 microns | 1.81 - 2.13 mil | ASTM D374 |
CEN® Electronic Material HT Polyimide Film CEN® HT is a one side or both sides electrically conductive polyimide film for heating applications. With precisely controlled surface resistivity, the film resistive property is retained througho.. |
|||
Thickness | 46.0 - 54.0 microns | 1.81 - 2.13 mil | ASTM D374 |
CEN® Electronic Material BL Polyimide Film CEN®BL polyimide film is a printable film that has the same thermal and chemical properties as CEN®CN Polyimide Film, which offers excellent performance in temperatures from -269-400°C. CEN®BL i.. |
|||
Thickness | 46.0 - 54.0 microns | 1.81 - 2.13 mil | |
CEN® Electronic Material CN Polyimide Film, 2 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Thickness | 46.0 - 54.0 microns | 1.81 - 2.13 mil | ASTM D374 |
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |