Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
Ovation Polymers OpteSTAT™ NC PP 0030 Polypropylene based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Surface Resistivity per Square | <= 10000 ohm | <= 10000 ohm | EOS/ESD S11.11 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Surface Resistivity per Square | 10000 - 20000 ohm @Thickness 1.57 mm |
10000 - 20000 ohm @Thickness 0.0620 in |
Condition A |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Surface Resistivity per Square | 10000 ohm | 10000 ohm | Applied Coating |
Heraeus Cleviosâ„¢ P T2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P T2 is an antistatic material based on PEDOT:.. |
|||
Surface Resistivity per Square | 10000 - 1.00e+7 ohm @Temperature 23.0 °C |
10000 - 1.00e+7 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Surface Resistivity per Square | <= 10000 ohm | <= 10000 ohm | |
Abatron AboCoat 8709-5 A/B Carbon-Filled Electrically Conductive Epoxy Compound AboCoat 8709-5 A/B is a high-solid carbon-epoxy coating with various conductivity ranges widely used in silk-screening. |
|||
Surface Resistivity per Square | <= 10000 ohm | <= 10000 ohm | IEC 60093 |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |