Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TI6500WV High Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI6500WV High Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High melt flow, superior low temperature impact, nucleated, good mold release, antistatic.Applications: Suggested uses include compounding, furniture, toys, packaging, large part injection molding, thin-walled injection molding.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 20.7 MPa
3000 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256A
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved